Continuous pH Monitoring During Pretreatment of Yellow Poplar Wood Sawdust by Pressure Cooking in Water
Yellow poplar wood sawdust consists of 41% cellulose and 19% hemicellulose. The goal of pressure cooking this material in water is to hydrate the more chemically resistive regio...