Related Publications
Metal Additive Manufacturing: A Review of Mechanical Properties
This article reviews published data on the mechanical properties of additively manufactured metallic materials. The additive manufacturing techniques utilized to generate sample...
Materials Synthesis by Mechanical Alloying
This article reviews published data on the mechanical properties of additively manufactured metallic materials. The additive manufacturing techniques utilized to generate sample...
Mechanical alloying — A perspective
Mechanical alloying is a dry, high energy ball milling process for producing composite metal powder with a fine controlled microstructure. It was originally developed to make hi...
An exploration of binder jetting of copper
Purpose – The purpose of this paper is to explore the use of binder jetting to fabricate high-purity copper parts. The ability to fabricate geometrically complex copper shapes w...
Effects of Melt Pool Variables and Process Parameters in Laser Direct Metal Deposition of Aerospace Alloys
Despite considerable advances in of laser direct metal deposition (LDMD) process optimization, there is rather limited work reported on the effects of melt pool variables on the...
Publication Info
- Year
- 2025
- Type
- article
- Volume
- 231
- Pages
- 115888-115888
- Citations
- 0
- Access
- Closed
External Links
Social Impact
Social media, news, blog, policy document mentions
Citation Metrics
Cite This
Identifiers
- DOI
- 10.1016/j.matchar.2025.115888