Luminescent CsPbI3 and Cs4PbI6 Aggregates in Annealed CsI:Pb Crystals
Luminescent aggregates of various types have been produced in quenched CsI:Pb single crystals by their annealing in vacuum at temperatures from 220 to 370 °C for 18 to 137 h. It...